Abstract
The mobility of strontium ions in these oxides is investigated at different temperatures by following the kinetics of its isotopic exchange under particle diffusion control conditions in order to study the effects of capacity, acidity, and porous texture on self-diffusion. Oxide preparation is described and detailed data for the apparent capacities and self-diffusion coefficients are presented.