Abstract
•Phototherapy on SBS of resin cement to zirconia ceramic was assessed.•Eight studies were included in the review.•Significant heterogeneity for SBS was noticed among phototherapy and control groups.•The overall mean difference for SBS was not significant between phototherapy and control.•Phototherapy on increasing SBS of resin cement to zirconia ceramic is debatable.
The present study systematically reviewed the literature to investigate the effect of phototherapy on the shear bond strength (SBS) of resin cement to zirconia ceramic.
Electronic databases including MEDLINE (PubMed), ISI Web of Science, Scopus, ScIELO, LILACS and EMBASE until April 2018. The addressed focused question was: Does phototherapy increase the SBS of resin cement to zirconia ceramics?”
A total of 8 in-vitro studies were included in the qualitative and quantitative analysis. The mean SBS for phototherapy ranged from 4.1 to 18.95 MPa while mean SBS for sandblasted zirconia-composite specimens ranged from 3.98 to 23.35 MPa in the included studies. Qualitative analysis showed 3 studies favoured application of phototherapy in significantly increasing SBS, while 4 studies indicated sandblasting showed significantly greater SBS of resin cement to zirconia ceramics. Considering the effects of phototherapy, significant heterogeneity for SBS (Q value = 136.37, p<0.0001, I2 = 94.87%) was noticed among both the groups. The overall mean difference for SBS (SMD = –0.59, 95% CI = –1.99 to –0.80, p = 0.402) was not significant between phototherapy and sandblast (control) groups.
Whether the effect of phototherapy on increasing the SBS of resin cement to zirconia ceramic is debatable. Further in-vitro studies should be performed in order to obtain strong conclusions.