Sign in
Mechanical properties of alpha-quartz using nanoindentation tests and molecular dynamics simulations
Journal article   Peer reviewed

Mechanical properties of alpha-quartz using nanoindentation tests and molecular dynamics simulations

Zhaoyang Ma, Ranjith Pathegama Gamage and Chengpeng Zhang
International journal of rock mechanics and mining sciences (Oxford, England : 1997), Vol.147, p.104878
01/11/2021

Abstract

Engineering Engineering, Geological Mining & Mineral Processing Physical Sciences Science & Technology Technology

Metrics

1 Record Views

Details