Optical and differential scanning calorimetry studies of the (Na2B4O7)-(CUO)-(CeO2) glass system
Journal article   Peer reviewed

Optical and differential scanning calorimetry studies of the (Na2B4O7)-(CUO)-(CeO2) glass system

A. A Kutub and A. S Shawoosh
Journal of materials science, Vol.32(20), pp.5491-5495
1997

Abstract

Condensed matter: electronic structure, electrical, magnetic, and optical properties Disordered solids Exact sciences and technology Infrared and raman spectra and scattering Optical properties and condensed-matter spectroscopy and other interactions of matter with particles and radiation Physics