Abstract
The conductivities of thin Al, Au, and Ag films were measured via their transmission at terahertz frequencies. The conductivities of all the films, particularly the thinner films and Al films, were much smaller than their bulk dc values. This reduced conductivity can be quantitatively understood in terms of an increased scattering rate from defects. The transmission is consistent with a frequency independent conductivity, implying a very fast electron scattering time.